Polymer Property : Volume Resistivity = 2.60e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity >= 2.60e+16 ohm-cm
>= 2.60e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific)
High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi.
Volume Resistivity >= 2.60e+16 ohm-cm
>= 2.60e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics Lexan® 4501 PPC
High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi.
Volume Resistivity 2.60e+16 ohm-cm
2.60e+16 ohm-cm
ASTM D257
Solvay Specialty Polymers Ajediumâ„¢ KT-820 Polyetheretherketone (PEEK)
KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu..
Volume Resistivity 2.60e+16 - 4.30e+16 ohm-cm
2.60e+16 - 4.30e+16 ohm-cm
ASTM D 257
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS
NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific ..
Volume Resistivity 2.60e+16 - 4.30e+16 ohm-cm
2.60e+16 - 4.30e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS
EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l..
Volume Resistivity 2.60e+16 ohm-cm

@Thickness 3.00 mm
2.60e+16 ohm-cm

@Thickness 0.118 in
IEC 60093
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..
Volume Resistivity 2.60e+16 - 3.60e+16 ohm-cm
2.60e+16 - 3.60e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Volume Resistivity 2.60e+16 - 3.60e+16 ohm-cm
2.60e+16 - 3.60e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Volume Resistivity 2.60e+16 - 3.60e+16 ohm-cm
2.60e+16 - 3.60e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Volume Resistivity 2.60e+16 - 3.60e+16 ohm-cm
2.60e+16 - 3.60e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Volume Resistivity 2.60e+16 - 3.60e+16 ohm-cm
2.60e+16 - 3.60e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL PX2060 PPE+PS
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Volume Resistivity 2.60e+16 - 3.60e+16 ohm-cm
2.60e+16 - 3.60e+16 ohm-cm
IEC 60093
SABIC Innovative Plastics NORYL PX2060 PPE+PS
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..