Solvay Specialty Polymers Ajediumâ„¢ KT-820 Polyetheretherketone (PEEK)

Category Polymer , Film , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Solvay Specialty Polymers
Trade Name Ajedium™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ajediumâ„¢ KT-820 Polyetheretherketone (PEEK).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high purity, and excellent chemical resistance to organics, acids, and bases. These properties make it well-suited for applications in aerospace, electronics, chemical processing, healthcare, transportation, and other industrial uses.Features: Ductile; Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; Good Impact Resistance; Good Sterilizability; High Heat Resistance; Radiation (Gamma) ResistantUses: Aircraft Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Medical/Healthcare Applications; Oil/Gas ApplicationsAdditional Properties: Area Factor - 149 ft²/lb/milInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ISO 62
Thickness 25.0 microns
0.984 mil
As Tested
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 75.8 MPa
11000 psi
ASTM D882
Film Tensile Strength at Yield, TD 72.4 MPa
10500 psi
ASTM D882
Film Elongation at Break, MD 150 %
150 %
ASTM D882
Film Elongation at Break, TD 170 %
170 %
ASTM D882
Film Elongation at Yield, MD 6.8 %
6.8 %
ASTM D882
Film Elongation at Yield, TD 6.7 %
6.7 %
ASTM D882
Secant Modulus, MD 2.05 GPa
297 ksi
ASTM D882
Secant Modulus, TD 2.00 GPa
290 ksi
ASTM D882
Dart Drop Test 390 g
0.860 lb
ASTM D1709
Film Tensile Strength at Break, MD 109 MPa
15800 psi
ASTM D882
Film Tensile Strength at Break, TD 95.8 MPa
13900 psi
ASTM D882
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
23.9 µin/in-°F

@Temperature -58.0 - 122 °F
1
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 340 °C
644 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 157 °C

@Thickness 3.20 mm
315 °F

@Thickness 0.126 in
Annealed; ASTM D648
Glass Transition Temp, Tg 150 °C
302 °F
DSC
Oxygen Index 37 %
37 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 2.60e+16 ohm-cm
2.60e+16 ohm-cm
ASTM D257
Surface Resistance >= 1.90e+17 ohm
>= 1.90e+17 ohm
ASTM D257
Dielectric Constant 3.05

@Frequency 1.00e+6 Hz
3.05

@Frequency 1.00e+6 Hz
ASTM D150
3.06

@Frequency 60.0 Hz
3.06

@Frequency 60.0 Hz
ASTM D150
3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 150 kV/mm

@Thickness 3.00 mm
3810 kV/in

@Thickness 0.118 in
ASTM D149
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Color Translucent
RoHS Compliance RoHS Compliant