Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.60e+14 ohm-cm | 1.60e+14 ohm-cm | |
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet.. |
|||
Volume Resistivity | 1.60e+14 ohm-cm | 1.60e+14 ohm-cm | |
Momentive Performance Materials RTV31 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
Volume Resistivity | 1.60e+14 ohm-cm | 1.60e+14 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and exc.. |
|||
Volume Resistivity | 1.60e+14 ohm-cm | 1.60e+14 ohm-cm | |
Dow Corning HV 1650/50 SILICONE RUBBER 50 Shore A hardness high consistency silicone rubber with excellent tracking and erosion resistance and low modulusInformation provided by Dow Corning |
|||
Volume Resistivity | <= 1.60e+14 ohm-cm | <= 1.60e+14 ohm-cm | |
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Volume Resistivity | <= 1.60e+14 ohm-cm | <= 1.60e+14 ohm-cm | |
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Volume Resistivity | 1.60e+14 ohm-cm | 1.60e+14 ohm-cm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon 35N Fast Cure Polyimide Laminate and Prepreg High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi.. |