Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 1.60e+14 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+14 ohm-cm
1.60e+14 ohm-cm
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite
Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet..
Volume Resistivity 1.60e+14 ohm-cm
1.60e+14 ohm-cm
Momentive Performance Materials RTV31 Silicone Rubber Compound for High Temperature, Red
RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa..
Volume Resistivity 1.60e+14 ohm-cm
1.60e+14 ohm-cm
ASTM D257
Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and exc..
Volume Resistivity 1.60e+14 ohm-cm
1.60e+14 ohm-cm
Dow Corning HV 1650/50 SILICONE RUBBER
50 Shore A hardness high consistency silicone rubber with excellent tracking and erosion resistance and low modulusInformation provided by Dow Corning
Volume Resistivity <= 1.60e+14 ohm-cm
<= 1.60e+14 ohm-cm
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Volume Resistivity <= 1.60e+14 ohm-cm
<= 1.60e+14 ohm-cm
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Volume Resistivity 1.60e+14 ohm-cm
1.60e+14 ohm-cm
C96/35/90; IPC TM-650 2.5.17.1
Arlon 35N Fast Cure Polyimide Laminate and Prepreg
High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi..
Copyright © lookpolymers.com All Rights Reserved