Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK)

Category Polymer , Film , Thermoplastic , Polyketone
Manufacturer Solvay Specialty Polymers
Trade Name Ajedium™ Films -- AvaSpire®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and excellent chemical resistance to organics, acids, and bases. These properties make it well-suited for applications in aerospace, electronics, transportation, chemical processing, and other industrial uses.Features: Ductile; Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; Good Impact Resistance; Good Sterilizability; High Heat Resistance; Radiation (Gamma) ResistantUses: Aircraft Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Medical/Healthcare Applications; Oil/Gas ApplicationsInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ISO 62
Thickness 50.0 microns
1.97 mil
As Tested
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 71.7 MPa
10400 psi
ASTM D882
Film Tensile Strength at Yield, TD 68.9 MPa
9990 psi
ASTM D882
Film Elongation at Break, MD 130 %
130 %
ASTM D882
Film Elongation at Break, TD 130 %
130 %
ASTM D882
Film Elongation at Yield, MD 5.0 %
5.0 %
ASTM D882
Film Elongation at Yield, TD 5.0 %
5.0 %
ASTM D882
Secant Modulus, MD 2.04 GPa
296 ksi
ASTM D882
Secant Modulus, TD 2.00 GPa
290 ksi
ASTM D882
Dart Drop Test 830 g
1.83 lb
ASTM D1709
Film Tensile Strength at Break, MD 86.9 MPa
12600 psi
ASTM D882
Film Tensile Strength at Break, TD 83.4 MPa
12100 psi
ASTM D882
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
23.9 µin/in-°F

@Temperature -58.0 - 122 °F
1
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 340 °C
644 °F
ASTM D3418
Glass Transition Temp, Tg 158 °C
316 °F
DSC
Oxygen Index 48 %
48 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+14 ohm-cm
1.60e+14 ohm-cm
ASTM D257
Surface Resistance >= 1.90e+17 ohm
>= 1.90e+17 ohm
ASTM D257
Dielectric Constant 3.05

@Frequency 1.00e+6 Hz
3.05

@Frequency 1.00e+6 Hz
ASTM D150
3.06

@Frequency 60.0 Hz
3.06

@Frequency 60.0 Hz
ASTM D150
3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 200 kV/mm

@Thickness 0.0500 mm
5080 kV/in

@Thickness 0.00197 in
ASTM D149
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Color Translucent
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: