Polymer Property : Volume Resistivity = 0.00060 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 0.00060 ohm-cm
0.00060 ohm-cm
Cured: 15 minutes at 25°C
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth..
Volume Resistivity 0.00060 ohm-cm
0.00060 ohm-cm
cured 5 min @ 160°C
Tra-Con Tra-Duct 2916 Room Temperature Conductive Silver Epoxy Adhesive
TRA-DUCT 2916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good ele..
Volume Resistivity 0.00060 ohm-cm
0.00060 ohm-cm
Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Emerson & Cuming 57C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy AdhesiveSilver filled, electrically conductive, room temperature curing, epoxy adhesive. Good thermal conduc..
Volume Resistivity 0.00060 ohm-cm
0.00060 ohm-cm
cured 1 hr @ 110°C
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive
TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop..