Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 57C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy AdhesiveSilver filled, electrically conductive, room temperature curing, epoxy adhesive. Good thermal conductivity. Convenient 1:1 mix ratio by weight or volume. Adheres to a wide variety of substrates. Recommended for use in applications where hot soldering is impractical. Mix ratio of 100:100. Cure Type: Room Temperature Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 3.50 g/cc
0.126 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 4.83 MPa
700 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.00060 ohm-cm
0.00060 ohm-cm
Processing Properties Metric English Comments
Cure Time 45.0 min

@Temperature 100 °C
0.750 hour

@Temperature 212 °F
180 min

@Temperature 65.0 °C
3.00 hour

@Temperature 149 °F
960 min

@Temperature 25.0 °C
16.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Silver
Viscosity Thixotropic Paste (Mixed, 25°C)