Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 9.90 kV/mm | 251 kV/in | Step by Step; ASTM D149 |
Plenco 08122 Polyester BMC, Compression Molded PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Dielectric Strength | 9.90 kV/mm | 251 kV/in | Short Time; ASTM D149 |
Plenco 2369 Phenolic, Granular, Injection Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |