Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Resole, Wood Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2369 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369 offers excellent physical and electrical strength properties. UL recognized under component file E40654. 02369 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.63 %
0.63 %
ASTM D570
Linear Mold Shrinkage 0.0084 cm/cm
0.0084 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 71
71
ASTM D785
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 1.02 %
1.02 %
ASTM D638
Tensile Modulus 7.40 GPa
1070 ksi
ASTM D638
Flexural Strength 88.0 MPa
12800 psi
ASTM D790
Flexural Modulus 6.60 GPa
957 ksi
ASTM D790
Compressive Strength 182 MPa
26400 psi
ASTM D695
Poissons Ratio 0.36
0.36
ASTM D638
Shear Modulus 2.72 GPa
395 ksi
Calculated
Izod Impact, Notched 0.166 J/cm
0.311 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.182 J/cm²
0.866 ft-lb/in²
ASTM D256
Impact 111
111
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 57.0 µm/m-°C

@Temperature 40.0 - 130 °C
31.7 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 186 °C
367 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Shrinkage 0.58 %
0.58 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+13 ohm-cm
1.20e+13 ohm-cm
ASTM D247
Dielectric Constant 5.7
5.7
ASTM D150
Dielectric Strength 9.90 kV/mm
251 kV/in
Short Time; ASTM D149
Dissipation Factor 0.056
0.056
ASTM D150
Arc Resistance 135 sec
135 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638