Polymer Property : Dielectric Strength = 251 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 9.90 kV/mm
251 kV/in
Step by Step; ASTM D149
Plenco 08122 Polyester BMC, Compression Molded
PLENCO 08122 is a renumber of PlasGlas 10212. PLENCO 08122 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..
Dielectric Strength 9.90 kV/mm
251 kV/in
Short Time; ASTM D149
Plenco 2369 Phenolic, Granular, Injection Molded
PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369..