Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.00 - 9.00 kV/mm @Temperature 90.0 °C |
178 - 229 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Dielectric Strength | 7.00 - 9.00 kV/mm @Temperature 90.0 °C |
178 - 229 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa.. |
|||
Dielectric Strength | 7.00 - 9.00 kV/mm @Temperature 90.0 °C |
178 - 229 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |