Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Amity Thermosets
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railway signaling equipment parts Kitchen equipment ( e.g. mixers, dishwashers ) parts Components which ought to have good electric insulation in spite of exposure to humid atmosphere, etc.Information provided by Amity Thermosets Limited
Physical Properties Metric English Comments
Density 1.40 - 1.46 g/cc
0.0506 - 0.0527 lb/in³
Molding; IS 867-1963
Apparent Bulk Density 0.200 - 0.300 g/cc
0.00723 - 0.0108 lb/in³
IS 867-1963
Water Absorption 0.12 - 0.22 %
0.12 - 0.22 %
IS 13411-1993
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
IS 13411-1992
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 - 55.0 MPa
6670 - 7980 psi
5 mm/min.; IS 867-1963
Shear Strength 70.0 - 80.0 MPa
10200 - 11600 psi
2mm/min.; IS 867-1963
Izod Impact, Notched 0.250 - 0.300 J/cm
0.468 - 0.562 ft-lb/in
IS 13411-1992
Electrical Properties Metric English Comments
Volume Resistivity 3.16e+11 - 3.16e+12 ohm-cm
3.16e+11 - 3.16e+12 ohm-cm
IS 3396-1979
Surface Resistance 1.00e+11 - 1.00e+12 ohm
1.00e+11 - 1.00e+12 ohm
IS 3396-1979
Dielectric Strength 7.00 - 9.00 kV/mm

@Temperature 90.0 °C
178 - 229 kV/in

@Temperature 194 °F
IS 2584-1963
Processing Properties Metric English Comments
Mold Temperature 160 - 180 °C
320 - 356 °F
Injection Pressure 14.7 - 39.2 MPa
2130 - 5690 psi
Mold Pressure
Cure Time 1.50 - 1.83 min
0.0250 - 0.0306 hour
per mm
Shelf Life 12.0 Month
12.0 Month
10-25°C