Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.00 - 48.0 kV/mm | 178 - 1220 kV/in | Average value: 28.9 kV/mm Grade Count:34 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Dielectric Strength | 7.00 - 37.0 kV/mm | 178 - 940 kV/in | Average value: 26.0 kV/mm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Dielectric Strength | 7.00 - 25.0 kV/mm | 178 - 635 kV/in | Average value: 11.2 kV/mm Grade Count:7 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Dielectric Strength | 7.00 - 50.0 kV/mm | 178 - 1270 kV/in | Average value: 29.0 kV/mm Grade Count:6 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | 60°C for 500 hrs |
Fujipoly Industries Sarcon® 30GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 30GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | AC 60 Hz; 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 30Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | 60°C for 500 hrs |
Fujipoly Industries Sarcon® 45T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | |
LG Chemical TR557 MABS, High Transparency, High Impact Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | AC Rapid Rise; ASTM D149 |
DuPont™ Nomex® N196 Paper, 5 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Dielectric Strength | 7.00 kV/mm | 178 kV/in | IEC 60243-1 |
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Dielectric Strength | 7.00 - 9.00 kV/mm @Temperature 90.0 °C |
178 - 229 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Dielectric Strength | 7.00 - 9.00 kV/mm @Temperature 90.0 °C |
178 - 229 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa.. |
|||
Dielectric Strength | 7.00 - 8.00 kV/mm | 178 - 203 kV/in | ASTM D149 |
Adamas Adalon® 453 PTFE, Mica filler Information provided by Adamas, HPM |
|||
Dielectric Strength | >= 7.00 kV/mm @Temperature 90.0 °C |
>= 178 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation
Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche.. |
|||
Dielectric Strength | 7.00 - 9.00 kV/mm @Temperature 90.0 °C |
178 - 229 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |