Material Notes:
PC0787 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0787 contains flame retardant additives to reduce normal flame spread characteristics so as to achieve a VW-1 flame resistance rating when tested according to the UL 44 Vertical Flame test on 14 AWG/45Mils wires. PC0787 contains a slower peroxide and therefore provides wider processing latitude. It is recommended for control cable insulation. Specifications: Underwriters Laboratories Standards 44 and 854.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 11.8 MPa
>= 1710 psi
after aging (168h, 150°C); ASTM D412
13.1 MPa
1900 psi
ASTM D412
Elongation at Break 275 %
275 %
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 27 %
27 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Dielectric Constant 2.75

@Frequency 60000 Hz
2.75

@Frequency 60000 Hz
ASTM D150
Dielectric Strength >= 550 kV/mm
>= 14000 kV/in
ASTM D149
Dissipation Factor 0.0026

@Frequency 60000 Hz
0.0026

@Frequency 60000 Hz
ASTM D150
Processing Properties Metric English Comments
Middle Barrel Temperature 116 - 127 °C
241 - 261 °F
Shelf Life 12.0 Month
12.0 Month