Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 18.4 kV/mm
467 kV/in
Short Time; ASTM D149
Plenco 6343 Phenolic, Granular, Transfer Molded
PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz..
Dielectric Strength 18.4 kV/mm
467 kV/in
Arlon SQA-TMS-020
Arlon 55578XA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty..