Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.4 kV/mm | 467 kV/in | Short Time; ASTM D149 |
Plenco 6343 Phenolic, Granular, Transfer Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Dielectric Strength | 18.4 kV/mm | 467 kV/in | Arlon SQA-TMS-020 |
Arlon 55578XA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty.. |