Plenco 6343 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6343 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recognized under component file E40654. 06343 is available in natural color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.810 g/cc
0.0293 lb/in³
ASTM D1895
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Water Absorption 0.044 %
0.044 %
ASTM D570
Linear Mold Shrinkage 0.0033 cm/cm
0.0033 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 77
77
ASTM D785
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 0.31 %
0.31 %
ASTM D638
Tensile Modulus 14.9 GPa
2160 ksi
ASTM D638
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
Flexural Modulus 14.1 GPa
2050 ksi
ASTM D790
Compressive Strength 173 MPa
25100 psi
ASTM D695
Poissons Ratio 0.279
0.279
ASTM D638
Shear Modulus 5.82 GPa
844 ksi
Calculated
Izod Impact, Notched 0.173 J/cm
0.324 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.212 J/cm²
1.01 ft-lb/in²
ASTM D256
Impact 84
84
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 21.0 µm/m-°C

@Temperature 40.0 - 130 °C
11.7 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 216 °C
421 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
365 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 43 %
43 %
ASTM D2863
Shrinkage 0.047 %
0.047 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 5.80e+12 ohm-cm
5.80e+12 ohm-cm
ASTM D247
Dielectric Constant 4.9
4.9
ASTM D150
Dielectric Strength 15.6 kV/mm
396 kV/in
Step by Step; ASTM D149
18.4 kV/mm
467 kV/in
Short Time; ASTM D149
Dissipation Factor 0.034
0.034
ASTM D150
Arc Resistance 183 sec
183 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638