Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.6 kV/mm | 524 kV/in | ASTM D149 |
3M Scotchcast™ 2104 Electrical Insulating Resin Scotchcast 2104 Electrical Insulating Resin is a hard, two-part, polyurethane resin encapsulant designed especially for permanent splice protection. 2104 is formulated for virtually every electrical.. |
|||
Dielectric Strength | 20.6 kV/mm | 522 kV/in | ASTM D149 |
Arlon RBLW401R##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths. ## in the product number indicates roll length in yards.. |
|||
Dielectric Strength | 20.6 kV/mm | 522 kV/in | ASTM D149 |
Arlon RBLW401X##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths. ## in the product number indicates roll length in yards.. |