Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchcast™ 2104 Electrical Insulating Resin

Category Other Engineering Material
Manufacturer 3M
Trade Name Scotchcast™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcast™ 2104 Electrical Insulating Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchcast 2104 Electrical Insulating Resin is a hard, two-part, polyurethane resin encapsulant designed especially for permanent splice protection. 2104 is formulated for virtually every electrical application requiring a hard, non-reenterable resin with good handling and performance characteristics. 2104 is also used as the insulating material for cable splices operating at 1000 volts or less and is rated for continuous use at 90°C with an overload rating 130°C. It may be stocked to cover all hard resin needs, ending the need for multiple encapsulant inventories. This resin is a two-part polyurethane, and is formulated with excellent wetting properties and low viscosity. 2104 flows well, even at low temperatures, filling the closure completely and eliminating voids. Cure time is fast; approximately one hour at 22°C and 20 hours at -4°C.Information provided by 3M
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Moisture Absorption 0.280 %
0.280 %
7 days at RT
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 3.06 MPa
444 psi
ASTM D412
Elongation at Break 98 %
98 %
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air 90.0 °C
194 °F
Glass Transition Temp, Tg -70.0 °C
-94.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 100 Hz,
Temperature 23.0 °C
3.8

@Frequency 100 Hz,
Temperature 73.4 °F
ASTM D150
Dielectric Strength 20.6 kV/mm
524 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 21.0 °C
1.00 hour

@Temperature 69.8 °F
1200 min

@Temperature -4.00 °C
20.0 hour

@Temperature 24.8 °F
Gel Time 18.0 min
18.0 min
Descriptive Properties Value Comments
Appearance Green
Users viewing this material also viewed the following: