Electrical Properties Metric English Comments
Dielectric Strength 6.70 kV/mm

@Thickness 3.00 mm
170 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Tubes
Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig..
Dielectric Strength 6.70 kV/mm

@Thickness 3.00 mm
170 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola Etronit IV C S Phenolic, Paper Reinforcement, Black, Tubes
Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig..
Dielectric Strength 6.70 kV/mm

@Thickness 3.00 mm
170 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Tubes
Description: Used in mechanical, electrical and electronic applications at elevated temperatures. Retains good electrical properties at high temperatures. Self-extinguishing. Low dielectric loss fac..