Material Notes:
Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at high frequencies.Information provided by Elektro-Isola
Physical Properties Metric English Comments
Density 1.25 g/cc

@Thickness >=0.000 mm
0.0452 lb/in³

@Thickness >=0.000 in
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3
Water Absorption 0.20 %
0.20 %
24hr/50°C+24hr in water at 23°C; ISO 62-1; IEC/EN 61212-2 7.2
Mechanical Properties Metric English Comments
Flexural Strength 120 MPa

@Diameter >=100 mm
17400 psi

@Diameter >=3.94 in
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1
Compressive Strength 130 MPa

@Temperature 23.0 °C,
Time 86400 sec
18900 psi

@Temperature 73.4 °F,
Time 24.0 hour
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Adhesive Bond Strength 145 MPa

@Diameter <=100 mm
21000 psi

@Diameter <=3.94 in
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 120 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Electrical Properties Metric English Comments
Insulation Resistance 2.00e+8 ohm

@Diameter 8.00 - 10.0 mm
2.00e+8 ohm

@Diameter 0.315 - 0.394 in
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2
Dielectric Constant 5.0

@Frequency 50.0 Hz
5.0

@Frequency 50.0 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
5.0

@Frequency 1.00e+6 Hz
5.0

@Frequency 1.00e+6 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
Dielectric Strength 6.70 kV/mm

@Thickness 3.00 mm
170 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
1.00 kV/mm

@Diameter >=3.00 mm
25.4 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Dissipation Factor 0.030

@Frequency 50.0 Hz
0.030

@Frequency 50.0 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
0.030

@Frequency 1000 Hz
0.030

@Frequency 1000 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3