Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled , Nylon 66, Heat Stabilized
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL File Number: E157318Appearance: Natural ColorTPCI# 8230101Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 137 MPa
19900 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 188 MPa
27200 psi
ASTM D790
Flexural Modulus 7.24 GPa
1050 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Thickness 3.17 mm
2.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
20.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Natural, black & colors
5VB

@Thickness 3.00 mm
5VB

@Thickness 0.118 in
Natural, black & colors
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
ASTM D257
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149