Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 6.60 kV/mm | 168 kV/in | Step by Step; ASTM D149 |
Plenco 4300 Phenolic, Granular, Injection Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Dielectric Strength | 6.60 kV/mm | 168 kV/in | Step by Step; ASTM D149 |
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Dielectric Strength | 6.60 - 14.9 kV/mm | 168 - 378 kV/in | Average value: 11.3 kV/mm Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |