Polymer Property : Dielectric Strength = 378 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 6.60 - 14.9 kV/mm
168 - 378 kV/in
Average value: 11.3 kV/mm Grade Count:5
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..