Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Melamine , Melamine-Phenolic Copolymer , Phenolic
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E40654. 00714 is available in brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.700 g/cc
0.0253 lb/in³
ASTM D1895
Density 1.67 g/cc
0.0603 lb/in³
ASTM D792
Water Absorption 0.275 %
0.275 %
ASTM D570
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 76
76
ASTM D785
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 0.57 %
0.57 %
ASTM D638
Tensile Modulus 11.8 GPa
1710 ksi
ASTM D638
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
Flexural Modulus 9.80 GPa
1420 ksi
ASTM D790
Compressive Strength 164 MPa
23800 psi
ASTM D695
Izod Impact, Notched 0.162 J/cm
0.303 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.199 J/cm²
0.947 ft-lb/in²
ASTM D256
Impact 81
81
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.580 W/m-K

@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 152 °C
306 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 202 °C
396 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 36 %
36 %
ASTM D2863
Shrinkage 0.69 %
0.69 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D247
Dielectric Constant 7.0
7.0
ASTM D150
Dielectric Strength 6.60 kV/mm
168 kV/in
Step by Step; ASTM D149
9.30 kV/mm
236 kV/in
Short Time; ASTM D149
Dissipation Factor 0.062
0.062
ASTM D150
Arc Resistance 186 sec
186 sec
ASTM D495
Comparative Tracking Index 475 V
475 V
ASTM D3638
Users viewing this material also viewed the following: