Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.0 - 16.0 kV/mm @Thickness 0.100 mm |
330 - 406 kV/in @Thickness 0.00394 in |
short term; ASTM D149 |
Polikim EFALON® C-25 PTFE, 25% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
Dielectric Strength | 13.4 - 16.0 kV/mm | 340 - 406 kV/in | Average value: 14.9 kV/mm Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Dielectric Strength | 7.87 - 16.0 kV/mm | 200 - 406 kV/in | Average value: 15.3 kV/mm Grade Count:11 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Dielectric Strength | 12.0 - 16.0 kV/mm | 305 - 406 kV/in | Average value: 13.7 kV/mm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Dielectric Strength | 15.0 - 16.0 kV/mm | 381 - 406 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories 99 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
Dielectric Strength | 15.0 - 16.0 kV/mm | 381 - 406 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories 99 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |