Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.78 - 15.75 kV/mm @Thickness 3.17 mm |
350.0 - 400.0 kV/in @Thickness 0.125 in |
Short time value |
Abatron AboCast/AboCure 8109-12 1-part, contains latent hardener activated by higher temperature. 4-6 month shelf life at 20-25°C (68-77°F). Other versions available with longer shelf lives and cure cycles.Processing: Potlife:.. |
|||
Dielectric Strength | 13.78 - 15.75 kV/mm @Thickness 3.17 mm |
350.0 - 400.0 kV/in @Thickness 0.125 in |
Short time value |
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |