Polymer Property : Dielectric Strength = 11.3 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 11.3 kV/mm
287 kV/in
Step by Step; ASTM D149
Plenco 1581 Polyester, Pellet, Injection Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..
Dielectric Strength 11.3 kV/mm
287 kV/in
Step by Step; ASTM D149
Plenco 1586 Polyester, Pellet, Transfer Molded
PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti..
Dielectric Strength 11.3 kV/mm
287 kV/in
Short Time; ASTM D149
Plenco 7500 Phenolic, Granular, Injection Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
Dielectric Strength 11.3 - 17.8 kV/mm
287 - 451 kV/in
Fluid Resistance, 24 hrs immersed; MIL-I-23053/15A
3M BBI-A Shrinkable Tubing for Bus Bar
3M Heat Shrinkable Tubing for Bus Bar BBI-A Series is designed for insulating rectangular, square and round bus bar rated from 5 kV through 35 kV. It will also cover and insulate inline bolted conne..
Dielectric Strength 11.3 kV/mm
287 kV/in
Short Time; ASTM D149
Plenco 4311 Phenolic, Granular, Transfer Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..