Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 1000 - 10000 ohm | 1000 - 10000 ohm | Average value: 4000 ohm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |