Electrical Properties Metric English Comments
Insulation Resistance 1000 - 10000 ohm
1000 - 10000 ohm
Average value: 4000 ohm Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..