Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 29.5 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 29.5 kV/mm

@Thickness 1.57 mm
750 kV/in

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S.T.
Industrial Laminates/Norplex NP130 Glass Fabric
Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic..
Dielectric Strength 29.5 kV/mm

@Thickness 1.57 mm
750 kV/in

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S.T.
Industrial Laminates/Norplex NP510A Glass Fabric
Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-..
Dielectric Strength 29.5 kV/mm

@Thickness 1.57 mm
750 kV/in

@Thickness 0.0620 in
Condition - A
Industrial Laminates/Norplex NP631 Paper Base Laminate
Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500"
Dielectric Strength 29.5 kV/mm

@Thickness 1.57 mm
750 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP680 Paper Base Laminate
Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500"
Dielectric Strength 29.5 kV/mm

@Thickness 1.57 mm
750 kV/in

@Thickness 0.0620 in
D-48/50
Industrial Laminates/Norplex P95 Glass Fabric
Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested..
Dielectric Strength 29.5 kV/mm

@Thickness 1.60 mm
749 kV/in

@Thickness 0.0630 in
in oil; ASTM D 149
SABIC Innovative Plastics Valox® 735 PBT
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re..
Dielectric Strength 29.5 kV/mm

@Thickness 1.60 mm
749 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific)
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.
Dielectric Strength 29.5 kV/mm

@Thickness 1.60 mm
749 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 735 PBT+PET
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.