Electrical Properties Metric English Comments
Dielectric Strength 2.80 kV/mm

@Thickness >=3.00 mm
71.1 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets
Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used i..
Dielectric Strength 2.80 kV/mm

@Thickness >=3.00 mm
71.1 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Dielectric Strength 2.80 kV/mm

@Thickness >=3.00 mm
71.1 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t..
Dielectric Strength 2.80 kV/mm

@Thickness >=3.00 mm
71.1 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V..
Dielectric Strength 2.80 kV/mm

@Thickness 3.17 mm
71.0 kV/in

@Thickness 0.125 in
100% RH for 96 hours; ASTM D149
Garlock BLUE-GARD® 3700 Compressed Aramid Fiber Gasketing, EPDM Binder
Aramid fiber, high-temperature fillers, and EPDM binder. For service areas with weak causticsExcellent SealabilityUnique blend of aramid fibers, fillers, and a EPDM rubber binder provides improved t..