Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets

Category Polymer , Thermoset , Phenolic
Manufacturer Elektro-Isola
Trade Name Etronax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used in high-voltage switchgear in which SF6 gas in used as the insulation mediumInformation provided by Elektro-Isola
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1
Water Absorption 0.27 %
0.27 %
24hr/50°C+24hr in water at 23°C,Test Specimen 50x50x3[mm]; ISO 62-1; IEC/EN 60893-2 8.2
Mechanical Properties Metric English Comments
Tensile Strength 135 MPa

@Thickness >=1.50 mm
19600 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Modulus of Elasticity 4.50 GPa

@Thickness >=1.50 mm
653 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Flexural Strength 150 MPa

@Thickness >=1.50 mm
21800 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Compressive Strength 450 MPa

@Thickness >=5.00 mm
65300 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Izod Impact, Notched (ISO) 50.0 kJ/m²

@Thickness >=5.00 mm
23.8 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 130 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
266 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Electrical Properties Metric English Comments
Insulation Resistance 1.00e+11 ohm

@Thickness >=3.00 mm
1.00e+11 ohm

@Thickness >=0.118 in
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3
Dielectric Constant 4.0

@Thickness <=3.00 mm,
Frequency 50.0 Hz
4.0

@Thickness <=0.118 in,
Frequency 50.0 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 60250; IEC/EN 60893-2 6.2
Dielectric Strength 2.80 kV/mm

@Thickness >=3.00 mm
71.1 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
20.0 kV/mm

@Thickness 3.00 mm
508 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Dissipation Factor 0.010

@Frequency 50.0 Hz
0.010

@Frequency 50.0 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 60250; IEC/EN 60893-2 6.2
Comparative Tracking Index 200 V

@Thickness 3.00 mm
200 V

@Thickness 0.118 in
IEC 60112; IEC/EN 60893-2 6.4