Polymer Property : Dielectric Strength = 15.7 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D 149
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific)
Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region.
Dielectric Strength 15.7 kV/mm

@Thickness 1.57 mm
400 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP310 Cotton Fabric
Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500".
Dielectric Strength 15.7 kV/mm

@Thickness 1.57 mm
400 kV/in

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S.T.
Industrial Laminates/Norplex NP509 Glass Fabric
Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc..
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 310 PBT
Unreinforced, general purpose. Typical viscosity 5000-7000.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 310 PBT
Unreinforced, general purpose. Typical viscosity 5000-7000.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific)
Unreinforced, general purpose. Typical viscosity 5000-7000.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific)
Unreinforced, general purpose. Typical viscosity 5000-7000.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 310HP PBT
PBT for compounding/fibers only. Not intended for injection molding. FDA compliant. Available in Natural color (1001) only.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 311 PBT
Unreinforced, improved resistance to UV. Medium viscosity.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D 149
SABIC Innovative Plastics Valox® 312 PBT
Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific)
Unreinforced, For compounding only (not for injection molding), Medium viscosity.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 315 PBT
Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 325 PBT
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 325 PBT
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific)
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
Dielectric Strength 15.7 kV/mm

@Thickness 3.20 mm
399 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific)
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.