Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310 PBT Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 310 PBT Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific) Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific) Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 310HP PBT PBT for compounding/fibers only. Not intended for injection molding. FDA compliant. Available in Natural color (1001) only. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 311 PBT Unreinforced, improved resistance to UV. Medium viscosity. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Valox® 312 PBT Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific) Unreinforced, For compounding only (not for injection molding), Medium viscosity. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 315 PBT Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific) General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.20 mm |
399 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific) General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |