Polymer Property : Shielding Effectiveness = 75 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 40 - 75 dB

@Frequency 1.00e+9 - 2.00e+9 Hz
40 - 75 dB

@Frequency 1.00e+9 - 2.00e+9 Hz
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating
Master Bond MB600SCN is an aqueous based, sodium silicate system with a silver coated nickel filler. It is intended for use in applications where very good shielding effectiveness is required and co..