Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating

Category Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond MB600SCN is an aqueous based, sodium silicate system with a silver coated nickel filler. It is intended for use in applications where very good shielding effectiveness is required and cost considerations might be more pronounced. Electromagnetic interference (EMI) and radio frequency interference (RFI) are very important factors in electronic applications. The energy emitted from various sources such as radios, appliances, etc. can interfere with other electronic devices that are made from plastics. Conductive coatings are often applied to the housings in order to protect the devices from these types of interferences. Key Features Very good shielding effectivenessTemperature resistance up to +700°FEasy applicationSilver coated nickel fillerCost effectiveInformation provided by MasterBond®
Physical Properties Metric English Comments
Specific Gravity 3.00 g/cc
3.00 g/cc
Solids Content 90 %
90 %
by weight
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 371 °C
700 °F
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Electrical Properties Metric English Comments
Surface Resistance <= 0.001 ohm
<= 0.001 ohm
Shielding Effectiveness 40 - 50 dB

@Frequency 7.00e+9 - 1.80e+10 Hz
40 - 50 dB

@Frequency 7.00e+9 - 1.80e+10 Hz
40 - 55 dB

@Frequency 2.00e+9 - 7.00e+9 Hz
40 - 55 dB

@Frequency 2.00e+9 - 7.00e+9 Hz
40 - 75 dB

@Frequency 1.00e+9 - 2.00e+9 Hz
40 - 75 dB

@Frequency 1.00e+9 - 2.00e+9 Hz
Processing Properties Metric English Comments
Cure Time 60.0 - 120 min

@Temperature >=79.4 °C
1.00 - 2.00 hour

@Temperature >=175 °F
1440 - 2880 min

@Temperature 23.9 °C
24.0 - 48.0 hour

@Temperature 75.0 °F
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers
Descriptive Properties Value Comments
Color light silver gray
Viscosity flowable thixotropic