Polymer Property : Shielding Effectiveness = 102 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 102 dB

@Frequency 2.00e+9 Hz
102 dB

@Frequency 2.00e+9 Hz
Mil-G-83528/Mil std 285
P & P Technology ECF-J Silver Aluminum Loaded Fluorosilicone
P & P Technology material reference ECF-J is a fluorosilicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical pro..
Shielding Effectiveness 102 dB

@Frequency 2.00e+9 Hz
102 dB

@Frequency 2.00e+9 Hz
Mil-G-83528/Mil std 285
P & P Technology EC-J Silver Aluminum Loaded Silicone
P & P Technology material reference EC-J is a silicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical properties..
Shielding Effectiveness >= 102 dB

@Frequency 1.00e+6 Hz
>= 102 dB

@Frequency 1.00e+6 Hz
H-Field
P & P Technology Oriented Wires In Silicone
P & P Technology SP, SS, SR, SW & SF Ranges of gasket materials consist of Monel or aluminum wires embedded into solid silicone, sponge silicone or fluorosilicone, a fire retardant variant is also a..
Shielding Effectiveness >= 102 dB

@Frequency 4.00e+8 Hz
>= 102 dB

@Frequency 4.00e+8 Hz
P-Field
P & P Technology Oriented Wires In Silicone
P & P Technology SP, SS, SR, SW & SF Ranges of gasket materials consist of Monel or aluminum wires embedded into solid silicone, sponge silicone or fluorosilicone, a fire retardant variant is also a..
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics COMBO® and COMBO® Strip Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel ..
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics Frame Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips Clamped in Aluminum ExtrusionsAvailable Forms: Strips, Fab. Lengths, Frames with Joined EMI Strips..Standard Metals Available in EMI Portion: Monel FerrexInf..
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics MESH STRIP™ (all metal) Wire Mesh EMI Gasket Selection Guide
Construction: Formed or Compressed Knitted Wire MeshAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Information provided by C..
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics METALASTIC® Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Woven Wire ElastomerAvailable Forms: Sheets, Die-Cut GasketsStandard Metals Available in EMI Portion: Aluminum OnlyInformation provided by Chomerics
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics POLASTRIP® Metal EMI Gasket
Description: POLASTRIP gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASTRIP gasketing, EMI shieldin..
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics PORCUPINE METALASTIC® Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Expanded Metal in ElastomerAvailable Forms: Sheets, Die-Cut GasketsStandard Metals Available in EMI Portion: Monel AluminumInformation provided by Chomerics
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics SHIELDMESH™ Wire Mesh EMI Gasket Selection Guide
Construction: Formed or Compressed Knitted Wire MeshAvailable Forms: Jointless Rings or Rectangular GasketsStandard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Information provided by Ch..
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics COMBO® Gaskets Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Die-Cut Elastomer with Joined EMI Strips.Standard Metals Available in EMI Portion: Mone..
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics MESH STRIP™ (Elastomer Core) Wire Mesh EMI Gasket Selection Guide
Construction: Knitted wire mesh over elastomer stripAvailable Forms: Strips, Gaskets Made by Joining Strips, Clip-On Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Informati..
Shielding Effectiveness >= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Parker Chomerics POLASHEET® Metal EMI Gasket
Description: POLASHEET gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASHEET gasketing individual mo..