Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 145 - 183 sec | 145 - 183 sec | Average value: 175 sec Grade Count:7 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Arc Resistance | 87.0 - 183 sec | 87.0 - 183 sec | Average value: 144 sec Grade Count:9 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |