Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 145 sec | 145 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N5000-30/32 BT Epoxy Package The Nelco N5000-30 prepreg and N5000-32 laminate BT epoxy materials are designed specifically to meet or exceed new and emerging chippackaging requirements. The primary applications of these materia.. |
|||
Arc Resistance | 145 sec | 145 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Arc Resistance | 145 sec | 145 sec | ASTM D495 |
Shell Carilon® DP R1130 Polyketone, 30% Glass Fiber Reinforced
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1130 is a 30 percent glass fiber reinforced compound based on a developmental e.. |
|||
Arc Resistance | 145 - 183 sec | 145 - 183 sec | Average value: 175 sec Grade Count:7 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Arc Resistance | 145 sec | 145 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Arc Resistance | 145 sec | 145 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Arc Resistance | 145 sec | 145 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic RX 611 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitomo.. |
|||
Arc Resistance | 145 sec | 145 sec | |
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Arc Resistance | 145 sec | 145 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Arc Resistance | 145 sec | 145 sec | ASTM D495 |
Sumitomo Bakelite North America RX® 790 Fiberglass Reinforced Phenolic Novolac RX 790 is a fiberglass reinforced phenolic novolac compound, featuring a good balance of strength and toughness. Information supplied by Sumitomo Bak North America. |
|||
Arc Resistance | 145 sec | 145 sec | |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |