Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 158 sec | 158 sec | ASTM D495 |
Eastman Eastar GN002 Copolyester, Natural
(discontinued **) Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Arc Resistance | 158 sec | 158 sec | IPC-TM-650.2.5.1 |
Park Electrochemical Nelco® N4000-7 EF® Halogen-Free Epoxy The Nelco® N4000-7 EF® series of laminates and prepregs is a total environmental solution. This advanced halogen-free resin system provides superior CAF resistance for high temperature, lead-free .. |
|||
Arc Resistance | 158 sec | 158 sec | ASTM D495 |
Plenco 4548 Phenolic, Granular, Injection Molded PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai.. |
|||
Arc Resistance | 158 sec | 158 sec | ASTM D495 |
Eastman Drystar 0113 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Arc Resistance | 158 sec | 158 sec | ASTM D495 |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Arc Resistance | 158 sec | 158 sec | ASTM D495 |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Arc Resistance | 158 sec | 158 sec | ASTM D495 |
Eastman GSP01 Copolyester for Film and Sheet Extrusion Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s.. |
|||
Arc Resistance | 158 sec | 158 sec | ASTM D495 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |