Material Notes:
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellent balance of properties such as superior aesthetics, impact strength, and chemical resistance. These properties can be optimally realized when the resins are properly dehydrated in accordance to recommended drying conditions and equipment.Recognizing this value, Eastman conceived DRYSTAR copolyesters to allow converters with limited access to desiccant dryers to achieve these optimizations. In addition, some converters with desiccant dryers may still find DRYSTAR copolyesters value-adding to attain production flexibility and cost saving by removing the drying process prior to injection molding, profile extruding, or extrusion blow molding copolyesters. The initial launch comprises of the commercialization of four grades of DRYSTAR copolyesters and Eastman has on-going program to extend this strategic product-line in the future.*DRYSTAR is only available in the Asia Pacific RegionApplications/UsesInjection molding
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Water Absorption 0.13 %
0.13 %
24h Immersion; ISO 62
0.13 %
0.13 %
24h Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0050 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength at Break 28.0 MPa
4060 psi
ISO 527
28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
50.0 MPa
7250 psi
ISO 527
Elongation at Break 60 %
60 %
ISO 527
110 %
110 %
ASTM D638
Elongation at Yield 4.2 %
4.2 %
ISO 527
4.3 %
4.3 %
ASTM D638
Flexural Yield Strength 68.0 MPa
9860 psi
ISO 178
70.0 MPa
10200 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ISO 178
2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm

@Temperature -40.0 °C
0.693 ft-lb/in

@Temperature -40.0 °F
ASTM D256
1.01 J/cm

@Temperature 23.0 °C
1.89 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 4.20 kJ/m²

@Temperature -40.0 °C
2.00 ft-lb/in²

@Temperature -40.0 °F
ISO 180
6.20 kJ/m²

@Temperature 23.0 °C
2.95 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Puncture Energy 12.0 J
8.85 ft-lb
Puncture Resistance @ max load, 23°C; ISO 6603-2
13.0 J

@Temperature -40.0 °C
9.59 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ISO 6603-2
Thermal Properties Metric English Comments
Specific Heat Capacity 1.30 J/g-°C

@Temperature 60.0 °C
0.311 BTU/lb-°F

@Temperature 140 °F
2.00 J/g-°C

@Temperature 240 °C
0.478 BTU/lb-°F

@Temperature 464 °F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ISO 75
70.0 °C
158 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ISO 75
64.0 °C
147 °F
ASTM D648
Vicat Softening Point 76.0 °C
169 °F
5kg load; ISO 306
85.0 °C
185 °F
1kg load; ISO 306
85.0 °C
185 °F
1kg load; ASTM D1525
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistivity per Square 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Constant 2.4

@Frequency 1e+6 Hz
2.4

@Frequency 1e+6 Hz
ASTM D150
2.6

@Frequency 1000 Hz
2.6

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.1 kV/mm
409 kV/in
Short Time, 500V/sec; ASTM D149
Dissipation Factor 0.0050

@Frequency 1000 Hz
0.0050

@Frequency 1000 Hz
ASTM D150
0.017

@Frequency 1e+6 Hz
0.017

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 158 sec
158 sec
ASTM D495
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 15.0 - 40.0 °C
59.0 - 104 °F
Drying Temperature 70.0 °C
158 °F
Dry Time 6 hour