Polymer Property : Surface Resistivity per Square = 8.00e+12 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 8.00e+12 ohm
8.00e+12 ohm
ASTM D257
Ovation Polymers Nemcon™ H ABS DP116P ABS
ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Surface Resistivity per Square 8.00e+12 ohm
8.00e+12 ohm
ASTM D257
Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy
Polycarbonate alloy-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Surface Resistivity per Square 8.00e+12 ohm
8.00e+12 ohm
ASTM D257
Ovation Polymers Nemcon™ H PC DP105/X3 BK Polycarbonate
Polycarbonate-Black colored, thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Surface Resistivity per Square 8.00e+12 ohm
8.00e+12 ohm
ASTM D257
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK
Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers