Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ovation Polymers
Trade Name Nemcon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate alloy-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.0 MPa
6820 psi
50 mm/min; ASTM D638
Elongation at Break 1.7 %
1.7 %
50 mm/min; ASTM D638
Tensile Modulus 3.175 GPa
460.5 ksi
50 mm/min; ASTM D638
Flexural Strength 75.0 MPa
10900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7.35 GPa
1070 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.187 J/cm

@Temperature 23.0 °C
0.350 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 3.50 W/m-K
24.3 BTU-in/hr-ft²-°F
ASTM E-1461
Deflection Temperature at 1.8 MPa (264 psi) 113 °C

@Thickness 3.20 mm
235 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 8.00e+12 ohm
8.00e+12 ohm
ASTM D257
Copyright © lookpolymers.com All Rights Reserved