Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ovation Polymers
Trade Name Nemcon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nemcon™ H PC DP105/X3 BK Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate-Black colored, thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 59.0 MPa
8560 psi
50 mm/min; ASTM D638
Elongation at Break 1.6 %
1.6 %
50 mm/min; ASTM D638
Tensile Modulus 6.90 GPa
1000 ksi
50 mm/min; ASTM D638
Flexural Strength 85.0 MPa
12300 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 8.20 GPa
1190 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.599 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 6.10 W/m-K
42.3 BTU-in/hr-ft²-°F
ASTM E-1461
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 8.00e+12 ohm
8.00e+12 ohm
ASTM D257