Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT 7048BK ABS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT 7048BK ABS Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT P048BK PP Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT R048BK PS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT R048BK PS Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Ensinger Tecaform™ SD Acetal (POM) Ensinger-Hyde static dissipative acetal contains no carbon fibers or powders and is generally accepted for clean room use. With its surface resistivity of 109 to 1011 ohm/square and its excellent b.. |
|||
Surface Resistivity per Square | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | ASTM D257 |
Ensinger Sintimid™ ESD 23 Polyamide-imide (PAI)
(discontinued **) SINTIMID™ ESD 23 has the highest compressive strength and use temperature of the group. It is based on an Ensinger-Hyde manufactured polyamide-imide resin with a low sloughing, additive package.In.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | ASTM D257 |
Kostat BK-STAT P048BK PP Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |