Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+8 ohm | 1.00e+8 ohm | ASTM D257 |
Kostat BK-STAT BK-STAT is an inherently dissipative polymer incorporated into a variety of resins as a melt additive. The electrical resistivity is reduced by formation of a conductive percolating network in the .. |
|||
Surface Resistivity per Square | 1.00e+8 - 1.00e+9 ohm | 1.00e+8 - 1.00e+9 ohm | ASTM D257 |
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide Melidin® 7021 CM is a self-lubricating compression molded polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best fo.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+8 ohm | 1e+05 - 1.00e+8 ohm | ASTM D257 |
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK) TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels.. |
|||
Surface Resistivity per Square | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | ASTM D257 |
Ensinger Sintimid™ ESD 23 Polyamide-imide (PAI)
(discontinued **) SINTIMID™ ESD 23 has the highest compressive strength and use temperature of the group. It is based on an Ensinger-Hyde manufactured polyamide-imide resin with a low sloughing, additive package.In.. |