Material Notes:
Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
(Dry)
Water Absorption 7.2 %
7.2 %
initially dry
Moisture Absorption at Equilibrium 2.1 %
2.1 %
initially dry
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Vicat Softening Point 195 °C

@Load 5.10 kg
383 °F

@Load 11.2 lb
50°C/h
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 350 V
350 V