Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.00e+17 ohm | 4.00e+17 ohm | ASTM D257 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Surface Resistance | 4.00e+17 ohm | 4.00e+17 ohm | ASTM D257 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI) Torlon® 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus w.. |
|||
Surface Resistance | >= 4.00e+17 ohm | >= 4.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Surface Resistance | 4.00e+17 - 5.00e+17 ohm | 4.00e+17 - 5.00e+17 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Surface Resistance | >= 4.00e+17 ohm | >= 4.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Surface Resistance | 4.00e+17 - 5.00e+17 ohm | 4.00e+17 - 5.00e+17 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Surface Resistance | >= 4.00e+17 ohm | >= 4.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Surface Resistance | 4.00e+17 - 5.00e+17 ohm | 4.00e+17 - 5.00e+17 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Surface Resistance | 4.00e+17 ohm | 4.00e+17 ohm | IEC 60093 |
Polyplastics Duranex® 7407 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |