Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.00e+17 - 5.00e+17 ohm | 4.00e+17 - 5.00e+17 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Surface Resistance | 4.00e+17 - 5.00e+17 ohm | 4.00e+17 - 5.00e+17 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Surface Resistance | 4.00e+17 - 5.00e+17 ohm | 4.00e+17 - 5.00e+17 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |